Component dosage /g component dosage /g
Addition products of A , epoxy resin and monoethanolamine (molecular weight 870 ) 21.3 B , epoxy resin 50
Addition of epoxy resin and diethyltriamine 35.9 Hardener solution 50
Butanol 8.6 xylene 80
Xylene 34.2 butanol 20
Preparation and curing   Mixing component A can produce epoxy resin hardener solution, and then mix with B component mixture to obtain adhesive, curing at 25 ° C. for 24 hours .
use   The adhesive can be cured at room temperature without irritating odor, has good heat resistance and moisture resistance, and is used for the bonding of building structural materials.
संपर्क करें

Author:

Ms. helen lu

ईमेल:

helenlu2007@gmail.com

Phone/WhatsApp:

++86 15073107995

लोकप्रिय उत्पाद
You may also like
Related Categories

इस आपूर्तिकर्ता को ईमेल

विषय:
ईमेल:
संदेश:

Your message must be betwwen 20-8000 characters

  • जांच भेजें

कॉपीराइट © सभी अधिकार सुरक्षित 2024 Hunan Magpow Adhesive Group co.,ltd।

We will contact you immediately

Fill in more information so that we can get in touch with you faster

Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.

भेजें